Free-Cutting Brass, UNS C36000, H02 (Cold Drawn 20% ) Temper 25 mm rod Categories: Metal; Nonferrous Metal; Copper Alloy; Brass Material Notes:

Fair to excellent corrosion resistance. Excellent machinability. Fabricated by machining, roll threading and knurling. Applications: gears, pinions, automatic high-speed screw machine parts. Test specimen: rod - 25mm diameter.

Key Words: free cutting, FC, CDA 360, CZ124, ISO CuZn36Pb3, CEN CW603N, FED QQ-B-626 (discontinued), ASTM-B121, ASTM-B36, ASTM-B16/B16M, ASTM-B124 Vendors:

Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Physical Properties Density Mechanical Properties Hardness, Rockwell B Tensile Strength, Ultimate Tensile Strength, Yield Elongation at Break Reduction of Area Modulus of Elasticity Poissons Ratio Machinability Shear Modulus Shear Strength Electrical Properties Electrical Resistivity Thermal Properties CTE, linear Specific Heat Capacity Thermal

Metric

English

8.50 g/cc

0.307 lb/in³

Metric

English

78

78

400 MPa

58000 psi

310 MPa

Comments

45000 psi

@Strain 0.500 %

@Strain 0.500 %

25.0 % 50.0 % 97.0 GPa

25.0 % 50.0 % 14100 ksi

0.311 100 % 37.0 GPa 235 MPa

0.311 100 % 5370 ksi 34100 psi

Metric

English

0.00000660 ohm-cm

0.00000660 ohm-cm

Metric

English

20.5 µm/m-°C

11.4 µin/in-°F

0.380 J/g-°C

0.0908 BTU/lb-°F

115 W/m-K

798 BTU-in/hr-ft²-°F

@Temperature 20.0 °C

Comments

In 50 mm

UNS C36000 (free-cutting brass) = 100%

Comments

@Temperature 68.0 °F

@Temperature 20.0 - 300 °C @Temperature 68.0 - 572 °F

Comments

Conductivity Melting Point Solidus Liquidus

@Temperature 20.0 °C

Processing Properties Annealing Temperature Hot-Working Temperature Recrystallization Temperature Component Elements Properties Copper, Cu Iron, Fe Lead, Pb Other Zinc, Zn

885 - 900 °C 885 °C 900 °C

@Temperature 68.0 °F

1630 - 1650 °F 1630 °F 1650 °F

Metric

English

425 - 600 °C

797 - 1110 °F

700 - 800 °C

1290 - 1470 °F

330 °C

626 °F

Metric

English

60.0 - 63.0 %
View more...